Abstract
In this work, The Electrical behaviour of ZnO based varistor is improved. On using the classical proceeding for fabricating the ceramic for Electronic, we have prepared different samples with different oxide additives such as (Bi2O3, Nb2O5, MnO2, Co3O4, Cr2O3, NiO, Ce2O3, and La2O3). We have got several lots, each of one represents one sample. We have optimized the percentage of the impurity as following: On varying the impurity percentage, we have obtain different values of the nonlinearity coefficient (alpha) fpr every sample. The greatest value of, alpha, corresponding to the best value of the proportion of the impurity which will be used in the final composition. Finally, we have mixed all best values together so we got a new sample, Our results explore that the value of (alpha) in the new sample is increaseed Significantly to a value of(100 +/- 2) and the non-linear region of the I-V characteristic of the varistor was improved. (C) 2012 Published by Elsevier Ltd. Selection and/or review under responsibility of The MEDGREEN Society.
-
Kapsamı
Uluslararası
-
Type
Hakemli
-
Index info
WOS.ISTP
-
Language
English
-
Article Type
None