In this study, 4 layers of 5 mm thick slats obtained by sawing method from poplar wood were used. Plain woven GRFP with low density and grammage of 100 g/m(2) (Type I) and plain woven GRFP with high density and grammage of 200 g/m(2) (Type 2) were placed and glued between each layer. Polyvinyl acetate (PLAc-D4), Polyurethane (PU) and dual-component Epoxy (L285-resin and 1-1285-hardener) adhesives were used for gluing the layers. Strength values (bending and modulus of elasticity) between the obtained layers were investigated. As a result of the study, it was determined that epoxy glue has higher strength than polyurethane and polyvinyl acetate glues; Type 2 plain woven fabric has higher strength than Type I plain woven fabric; and parallel load to the glue line results in higher performance than perpendicular load to the glue line.

  • Kapsamı

    Uluslararası

  • Type

    Hakemli

  • Index info

    WOS.SCI

  • Language

    English

  • Article Type

    None

  • Keywords

    poplar wood laminate bending strength modulus of elasticity